1 General Description The described set-up is used to produce coated oxides such as titanium oxide (TiO2) through chemical vapour deposition (CVD) of silicon tetrachloride (SiCl4). An oxide is treated either in solid or in fluidized bed by silicon tetrachloride (SiCl4). After the compound is adsorbed it must be treated with water and finally calcinated with argon or air. The maximum temperature that the reaction can reach is 450°C (723 K). The system is heated by a furnace, in which Duran- or silica reactors are inserted. Currently the whole system is operating at atmospheric pressure. Attention: corrosive gases and corrosive liquids can be produced (SiCl4, HCl). If these corrosive materials leak from the system, corrosion can occur. The equipment is set under the hood and must be examined by experienced staff.